2017-07-18 来自: 济南地面找平服务团队 浏览次数:243
1、将搅拌好的HGM80倒出,均匀的铺开,用专用齿口刮板控制厚度,本品施工厚度 3mm,一
1, mix the HGM80 poured evenly spread, with special tooth mouth scraper control thickness, the thickness of the construction of a 3mm.
次施工厚度3~30mm,参考用量1.6kg/m/ mm。
The thickness of the construction of 3~30mm, the reference dosage mm 1.6kg/m/.
2、施工人员可穿好钉鞋进入施工地面,用齿口刮板将砂浆面层刮平,以消除倾倒衔接处的不平并
2, the construction personnel can be put into the construction of the ground with spikes, tooth mouth scraper will be mortar scraping, to eliminate the uneven and dumping of cohesion
保持所需的厚度。
Maintain the required thickness.
3、用放气滚筒轻轻滚动以消除搅拌时产生的气泡。
3, with the release roller gently rolling to eliminate the bubbles generated when stirring.
4、拌和好的HGM80应在35分钟内用完。
4, mixing good HGM80 should be used up within 35 minutes.