光固化地坪漆涂膜流平的解决方式

2017-07-18  来自: 济南地面找平服务团队 浏览次数:881

光固化地坪漆涂料的稀释剂与挥发型涂料的稀释剂极不相同,挥发型涂料是靠稀释剂挥发后形成涂膜的,也就是说挥发性环氧地坪漆涂料干涂膜是没有稀释剂的。
Light curing floor paint paint thinner and thinner volatile coating is very different, volatile coating is thinner after volatilization of forming a coating film, i.e. epoxy floor paint volatile dry film is not thinner.
而光固化涂料的稀释剂是活性稀释剂,亦即不易挥发的活性单体,它在地坪漆涂料成膜过程中参与聚合反应,成膜后成为涂膜的一部分,而没有向大气层挥发。
Light curing coatings diluent is a reactive diluent, less volatile active monomer and its film-forming process in the polymerization reaction in floor paint, after the film became a part of the film, but not to the atmosphere.
也就是说,光固化地坪漆涂料的稀释剂既是涂料稀释剂又是涂料的成膜物,所以其固体含量极高(90%以上),流动性相对较差。
That is to say, the thinner of the light curing floor paint coating is not only the paint thinner but also the film forming material, so the solid content is very high (above 90%), the fluidity is relatively poor.
由于光固化环氧地坪漆涂料的固化速度极快,在2-5秒内即可实干,固化期间根本没有流平机会,因此就会产生流平不良的现象。地坪漆公司处理此类问题的方法主要是在光固化涂料涂装后,不要马上进行固化,静置20-30分钟待涂膜流平后,再行固化就可解决流平不良的问题。
Due to the curing speed of the light curing epoxy floor paint coating is extremely fast, it can be hard work in 2-5 seconds, and there is no chance to flow at all during the solidification. Floor paint company to deal with such problems is mainly in light curing coating coating, do not immediately after curing, static 20-30 minutes to wait for the film flow, and then can solve the problem of flow.