地面找平砂浆自流平材料配制

2017-07-18  来自: 济南地面找平服务团队 浏览次数:308

1、小面积或公路施工时,可用小型电动搅拌器,在桶中进行搅拌,每搅拌一次需用完整包料;大面积施工时,可用高速搅拌机搅拌,用砂浆泵送的方法施工。
1, a small area or road construction, use a small electric mixer, stirring in the bucket, each stirring with one complete package material; the construction of large area, high speed mixer mixing available, with the construction method of mortar pump.
2、搅拌方法:将适量的清水或HGM-80增强液倒入桶中,开启搅拌器边搅拌边徐徐加入一包自流平,搅拌4~5min,静止约1min后,再次搅拌至均匀无团的浆状即可。寒冷的情况下,宜用温水(不超过40℃)搅拌。
2, mixing method: the right amount of water or HGM-80 reinforced liquid into the barrel, open the stirring edge of the blender and slowly add a pack of self leveling, stirring 4~5min, static about 1min, once again stirred to even without a group of slurry can be. Cold conditions, the appropriate use of warm water (not more than 40 degrees Celsius).
3、施工温度宜5℃以上,配制好的自流平砂浆宜在35min内用完。
3, construction temperature is more than 5 degrees Celsius, the preparation of good self leveling mortar should be used in the 35min.
4、将搅拌好的自流平倒出,均匀的铺开,用专用齿口刮板控制厚度,本品施工厚度≥3mm,一次施工厚度3~30mm,参考用量1.6kg/m2/mm。
4, mix the self leveling poured evenly spread, with special tooth mouth scraper control thickness, the thickness of 3mm construction, construction of a thickness of 3~30mm, the amount of reference 1.6kg/m2/mm.
5、施工人员可穿好钉鞋进入施工地面,用齿口刮板将砂浆面层刮平,以消除倾倒衔接处的不平,并保持所需的厚度。
5, the construction personnel can be put into the construction of the ground with spikes, tooth mouth scraper will be mortar scraping, to eliminate dumping at the junction of injustice, and maintain the required thickness.